Properties
| Trademark | Basic Material | Appearance | Grafting Level | Density(g/cm3) | 
| GT-RA | ABS | light yellow particles | Medium | 0.95-1.0 | 
 
Effects of GT-RA on the properties of toughened ABS
| Properties | Measurement | ABS | ABS+5%(GT-RA) | 
| Tensile Strength | MPa | 50 | 47 | 
| Bending strength | MPa | 72 | 68 | 
| Izod impact strength | KJ/m² | 18 | 24 | 
Note: The above data are typical laboratory results, true and reliable, for reference only, and do not make a formal quality commitment.